Fw: Stress
Jack Badenhorst ( (no email) )
Tue, 25 Aug 1998 08:24:38 +0200
-----Original Message-----
From: Jack Badenhorst <xrd@aec.co.za>
To: RIETVELD_L Distribution List <rietveld_l@ill.fr>
Cc: RIETVELD_L Distribution List <rietveld_l@ill.fr>
Date: 25 August 1998 08:23
Subject: Stress
>
>-
>> Hello
>I know this is a rietveld group, but I need some help with stress
>measurements. Is there someone that can help me I have just started in this
>field.
>
>Regards Jack Badenhorst
>AEC, South Africa
>