High temp PXRD
MARTIN VICKERS TEL: 0171 631 6813 ( vickers@gordon.cryst.bbk.ac.uk )
Tue, 9 Jun 1998 15:40:33 +0100
We are currently developing the high temp set-up for our D500. We already have
GTP and Linkham equipment, but want to include something like an Anton-Paar or
Buehler system. Does anyone have contact addresses/www sites/e-mail/tel.numbers
of these companies, or indeed any other companies that produce high temp
equipment for powder diffractometers.
All information gratefully received.
Martin Vickers,
Birkbeck Crystallography.