Lepidocrocite Structure
Diffract ( Diffract@aol.com )
Wed, 13 May 1998 22:44:30 EDT
Lepidocrocite, gamma-FeO(OH), is a rather important phase in ferrous corrosion
scenarios. Does anybody know of a more recent structural analysis than the one
referenced in Structure Reports 44A, 1978A (which does not relate well to real
world samples).
Thanks
L. Keller
CAMET Research, Inc.
Goleta, CA