Re: Guinier geometry and Rietveld
MARTIN VICKERS TEL: 0171 631 6813 ( vickers@gordon.cryst.bbk.ac.uk )
Fri, 13 Mar 1998 09:48:44 +0100
As far as I am aware, Rietveld analysis on Guinier data is not routine, mainly,
I suspect, because of the absorption problems. I would, however, be very
interested to hear from anyone who has attempted Rietveld on Guinier data.
Martin Vickers
Dept. of Crystallography
Birkbeck College
London