Hi All,
 
Can anybody advise me about the use of spherical harmonic for 
modelling the prefered orientation in Rietveld refinement using 
GSAS?
How many spherical harmonic terms should I use for obtaining a good fit?
 
Also: Is there any other method for modelling the prefered orientation 
besides the traditional Rietveld-Toraya and March-Dollase functions?
 