Hi Rietveld users,
I'm working in Rietveld refinements(dbws9411 version) for quantitative 
phase analysis of Zro2 at various concentrations of y2o3 
(2%mol-8.5%mol). The convergence for pseudo-Voight function in the T+C 
cases(4.5%-7%mol y203) is giving NA~2.
I'm trying to apply the split-PearsonVII function, but the outputs are 
just errors messages for the m values.
I need some suggestions for the initial values of NA,NB & NC, and other 
possible errors that could arise in the application of this function