...Are there any newish references around the place about the
validity of R Bragg in Rietveld ...
You can get quite nice Bragg R's purely becuase 20% to 80% of the intensity
that is being fitted relates to the background.  Thus are there any background
subtracted versions for Rietveld of Bragg R referenced in the literature?
Lachlan,
there was a paper in the early '90ies which treats the problem, I think it was
a french author in J Appl Cryst - helas, I can't specify you more as I am on 
leave from my hardware (paper) file of bibliographic references!
Regards
Miguel Gregorkiewitz