Re: zero point
Stanislaw Gierlotka ( xray@pl.waw.unipress.iris )
Wed, 28 Sep 94 20:06:46 +0200
I played the game described by Armel Le Bail with DBWS. The behaviour was
essentially the same i.e. R-WP up and then down but the result was:
zero: -0.2262
displ: 0.1998
My diffractometer is not that misaligned!
Conlusions:
1. The quality of the data remains the key point.
2. Looking at the peaks at the very end of the pattern helps to understand
   what the program does or can do.
3. Armel's result nevertheless looks convincing.
Stan Gierlotka
-------------------------+---------------------------------------
X-Ray Diffraction Lab.   I  High Pressure Research Centre
phone  + (48 22) 328497  I  Polish Academy of Sciences
 |                       I  Sokolowska 29, 01-142 Warszawa, Poland
 |                       I  phone (international) +(48) 3912 3276
 |      |                I  phone (local)         +(48 22) 325010
 |      |   |       |    I  fax (international)   +(48) 3912 0331
_|_|____|___|_|__|__||__ I  fax (local)           +(48 22) 324218
-------------------------+--------------------------------------